Properties Of Activated Alumina Spheres

Mar 23, 2022

Because of its unique pore structure, large specific surface area and activity, activated alumina ball has many properties different from other products. It is often used as adsorbent, desiccant and catalyst carrier for the purification of various gases and liquids. Its remarkable performance is as follows:

1. High specific surface area, 300-350m2 / g

2. Soak in water without softening, cracking, expansion and pulverization

3. Easy to regenerate and use, with a service life of more than 3 years

4. Very low wear rate, Less than or equal to 0.1 percent

5. Strong adsorption capacity, drying capacity and purification capacity

 